Poly(2,5-difluorostyrene)
CROW logo
Poly(2,5-difluorostyrene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyhalostyrene
COMMON NAMESPoly(2,5-difluorostyrene), Poly(1,4-difluoro-2-vinylbenzene)
STRUCTURE BASED NAME Poly[1-(2,5-difluorophenyl)ethane-1,2-diyl], Poly(2,5-difluorophenylethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(c1c(F)ccc(F)c1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 305371-97-5
COMMON NAMES2,5-Difluorostyrene
SMILES C=Cc1cc(F)ccc1F
Std. InChI 1S/C8H6F2/c1-2-6-5-7(9)3-4-8(6)10/h2-5H,1H2
Std. InChIKey DSIWLDCXHHMNQL-UHFFFAOYSA-N
STRUCTURE
Poly(2,5-difluorostyrene)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1106.0
Density ρg mL-1 0.96
Solubility Parameter δMPa1/2 17.0 - 18.717.7
Molar Cohesive Energy EcohJ mol-1 30600 - 3710033100
Glass Transition Temperature TgK 374
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 102.14
Van-der-Waals Volume VvWmL mol-1 65.56
Molar Volume VmmL mol-1106.0 - 117.7111.2
Density ρg mL-1 0.87 - 0.960.92
Solubility Parameter δMPa1/2 16.6 - 18.317.5
Molar Cohesive Energy EcohJ mol-1 32600 - 3550034200
Glass Transition Temperature TgK 386 - 391389
Molar Heat Capacity CpJ (mol K)-1121 - 156137
Entanglement Molecular Weight Meg mol-111000 - 2000016000
Index of Refraction nnone1.51 - 1.541.52