Poly(2-methoxystyrene)
CROW logo
Poly(2-methoxystyrene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polystyrenes
COMMON NAMESPoly(2-methoxystyrene)
STRUCTURE BASED NAME Poly[1-(2-methoxyphenyl)ethane-1,2-diyl], Poly(2-methoxyphenylethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(c1c(OC)cccc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 612-15-7
COMMON NAMES2-Methoxystyrene
SMILES C=Cc1ccccc1OC
Std. InChI 1S/C9H10O/c1-3-8-6-4-5-7-9(8)10-2/h3-7H,1H2,2H3
Std. InChIKey SFBTTWXNCQVIEC-UHFFFAOYSA-N
STRUCTURE
Poly(2-methoxystyrene)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1122.4
Density ρg mL-1 1.10
Solubility Parameter δMPa1/2 18.4 - 20.219.4
Molar Cohesive Energy EcohJ mol-1 41400 - 4990046200
Glass Transition Temperature TgK 348
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.57 - 1.591.59
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 134.18
Van-der-Waals Volume VvWmL mol-1 78.39
Molar Volume VmmL mol-1121.6 - 128.2125.0
Density ρg mL-1 1.05 - 1.101.07
Solubility Parameter δMPa1/2 18.6 - 19.419.2
Molar Cohesive Energy EcohJ mol-1 44100 - 4700046200
Glass Transition Temperature TgK 342 - 372357
Molar Heat Capacity CpJ (mol K)-1165 - 175169
Entanglement Molecular Weight Meg mol-120000 - 3200027000
Index of Refraction nnone1.55 - 1.571.56
back to top