Poly(2-ethoxyethyl methacrylate)
CROW logo
Poly(2-ethoxyethyl methacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylate
COMMON NAMESPoly(2-ethoxyethyl methacrylate)
STRUCTURE BASED NAME Poly(2-ethoxyethyl 2-methylpropenoate)
ACRONYMS PHEMA
CAS #
CurlySMILES C{-}C{n+}(C)(C(=O)OCCOCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 2370-63-0
COMMON NAMES2-Ethoxyethyl methacrylate
SMILES CCOCCOC(=O)C(=C)C
Std. InChI 1S/C8H14O3/c1-4-10-5-6-11-8(9)7(2)3/h2,4-6H2,1,3H3
Std. InChIKey SFPNZPQIIAJXGL-UHFFFAOYSA-N
STRUCTURE
Poly(2-ethoxyethyl methacrylate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1145.6
Density ρg mL-1 1.09
Solubility Parameter δMPa1/2 17.5 - 20.318.6
Molar Cohesive Energy EcohJ mol-1 43300 - 6000050100
Glass Transition Temperature TgK
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.48 - 1.511.50
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 158.20
Van-der-Waals Volume VvWmL mol-1 89.01
Molar Volume VmmL mol-1139.0 - 142.8141.3
Density ρg mL-1 1.11 - 1.141.12
Solubility Parameter δMPa1/2 18.3 - 19.118.7
Molar Cohesive Energy EcohJ mol-1 48000 - 5060049200
Glass Transition Temperature TgK 297
Molar Heat Capacity CpJ (mol K)-1281 - 311
226 - 241
303 (l,r)
234 (s)
Entanglement Molecular Weight Meg mol-128000 - 3300031000
Index of Refraction nnone1.48 - 1.491.48
back to top