Poly(1-bromo-1-butenylene)
CROW logo
Poly(1-bromo-1-butenylene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyhalodienes
COMMON NAMESPoly(1-bromo-1-butenylene)
STRUCTURE BASED NAME Poly(1-bromo-1,3-butadiene)
ACRONYMS
CAS #
CurlySMILES C{-}(Br)=CCC{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS #
COMMON NAMES1-Bromo-1-butenylene
SMILES BrC=CC=C
Std. InChI 1S/C4H5Br/c1-2-3-4-5/h2-4H,1H2
Std. InChIKey LKNKAEWGISYACD-UHFFFAOYSA-N
STRUCTURE
1-Bromo-1-butenylene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-178.0
Density ρg mL-1 1.70
Solubility Parameter δMPa1/2 18.1 - 19.218.8
Molar Cohesive Energy EcohJ mol-1 25300 - 2880027400
Glass Transition Temperature TgK 225 - 241233
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 132.99
Van-der-Waals Volume VvWmL mol-1 51.54
Molar Volume VmmL mol-172.5 - 76.874.7
Density ρg mL-1 1.73 - 1.831.78
Solubility Parameter δMPa1/2 19.3 - 19.819.5
Molar Cohesive Energy EcohJ mol-1 27700 - 2880028300
Glass Transition Temperature TgK 234 - 252243
Molar Heat Capacity CpJ (mol K)-1132 - 143134
Entanglement Molecular Weight Meg mol-17700 - 2100011000
Index of Refraction nnone1.57 - 1.621.60
back to top