Poly(tetrafluoropropyl methacrylate)
CROW logo
Poly(2,2,3,3-tetrafluoropropyl methacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylate
COMMON NAMES Poly(2,2,3,3-tetrafluoropropyl methacrylate)
STRUCTURE BASED NAME Poly(2,2,3,3-tetrafluoropropyl 2-methylpropenoate)
ACRONYMS  
CAS #  
CurlySMILES C{-}C{n+}(C)(C(=O)OCC(F)(F)C(F)F
 

IDENTIFIERS OF MONOMER(S)

CAS # 45102-52-1
COMMON NAMES 2,2,3,3-Tetrafluoropropyl methacrylate
SMILES FC(F)C(F)(F)COC(=O)C(=C)C
Std. InChI InChI=1S/C7H8F4O2/c1-4(2)5(12)13-3-7(10,11)6(8)9/h6H,1,3H2,2H3
Std. InChIKey RSVZYSKAPMBSMY-UHFFFAOYSA-N
STRUCTURE
Tetrafluoropropyl methacrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 122.5 
Density ρg mL-1 1.52 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK 339 - 353344
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.417 - 1.4221.42
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 186.1
Van-der-Waals Volume VvWmL mol-1 74.0
Molar Volume VmmL mol-1 114.8 - 122.5119.3
Density ρg mL-1 1.52 - 1.581.54
Solubility Parameter δMPa1/2 15.6- 16.716.2
Molar Cohesive Energy EcohJ mol-1 33600 - 3700035200
Glass Transition Temperature TgK 337- 345341
Molar Heat Capacity Cp J (mol K)-1 195 - 249233
Entanglement Molecular Weight Meg mol-1 25400 - 3280029000
Index of Refraction nnone 1.41 - 1.431.42

  Last updated: October 25, 2015