POLYMER CLASS | Polyacrylate |
COMMON NAMES | Poly(2,2,3,3-tetrafluoropropyl acrylate) |
STRUCTURE BASED NAME | Poly(2,2,3,3-tetrafluoropropyl propenoate) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(C(=O)OCC(F)(F)C(F)F |
CAS # | 7383-71-3 |
COMMON NAMES | 2,2,3,3-Tetrafluoropropyl acrylate |
SMILES | FC(F)C(F)(F)COC(=O)C(=C) |
Std. InChI | InInChI=1S/C6H6F4O2/c1-2-4(11)12-3-6(9,10)5(7)8/h2,5H,1,3H2 |
Std. InChIKey | VHJHZYSXJKREEE-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 122.5 | |
Density ρ | g mL-1 | 1.52 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 247 - 251 | 249 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.42 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 186.1 | |
Van-der-Waals Volume VvW | mL mol-1 | 74.0 | |
Molar Volume Vm | mL mol-1 | 115 - 122 | 119 |
Density ρ | g mL-1 | 1.52 - 1.58 | 1.54 |
Solubility Parameter δ | MPa1/2 | 16.0 - 16.9 | 16.5 |
Molar Cohesive Energy Ecoh | J mol-1 | 29700 - 33400 | 31500 |
Glass Transition Temperature Tg | K | 232 - 268 | 250 |
Molar Heat Capacity Cp | J (mol K)-1 | 260 - 285 | 270 |
Entanglement Molecular Weight Me | g mol-1 | 22900 - 26500 | 24700 |
Index of Refraction n | none | 1.40 - 1.42 | 1.41 |
Last updated: October 25, 2015