POLYMER CLASS | Polyphenylenes (Polyaromatics) |
COMMON NAMES | Poly(p-phenylene vinylene) |
STRUCTURE BASED NAME | Poly(1,4-phenylene-1,2-ethenediyl), Poly[1-(1,4-phenylene)ethylene] |
ACRONYMS | PPV |
CAS # | 26009-24-5 |
CurlySMILES | c1{-}ccc(cc1)C=C{n+} |
CAS # | 106-37-6, 74-85-1 |
COMMON NAMES | 1,4-Dibromobenzene, Ethylene |
SMILES | Brc1ccc(cc1)Br.C=C |
Std. InChI | 1S/C6H4Br2/c7-5-1-2-6(8)4-3-5/h1-4H.1S/C2H4/c1-2/h1-2H2 |
Std. InChIKey | SWJPEBQEEAHIGZ-UHFFFAOYSA-N.VGGSQFUCUMXWEO-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | ||
Density ρ | g mL-1 | ||
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 353 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.59 - 1.80 | 1.69 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 102.14 | |
Van-der-Waals Volume VvW | mL mol-1 | 63.7 | |
Molar Volume Vm | mL mol-1 | 92.5 - 98.1 | 95.2 |
Density ρ | g mL-1 | 1.04 - 1.10 | 1.07 |
Solubility Parameter δ | MPa1/2 | 18.8 - 19.6 | 19.2 |
Molar Cohesive Energy Ecoh | J mol-1 | 34100 - 36400 | 35200 |
Glass Transition Temperature Tg | K | 315 - 317 | 316 |
Molar Heat Capacity Cp | J (mol K)-1 | 116 - 130 (s) | 120.2 |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.60 - 1.69 | 1.65 |
Last updated: January 31, 2020