POLYMER CLASS | Polyesters |
COMMON NAMES | Poly(1,6-hexylene succinate) |
STRUCTURE BASED NAME | Poly(oxyhexane-1,6-diyloxybutanedioyl), Poly(oxyhexane-1,6-diyloxysuccinyl) |
ACRONYMS | |
CAS # | |
CurlySMILES | O{-}CCCCCCOC(=O)CCC{n+}(=O) |
CAS # | 203-740-4, 629-11-8 |
COMMON NAMES | Succinic acid, 1,6-Hexanediol |
SMILES | OC(=O)CCC(=O)O.OCCCCCCO |
Std. InChI | 1S/C4H6O4/c5-3(6)1-2-4(7)8/h1-2H2,(H,5,6)(H,7,8).1S/C6H14O2/c7-5-3-1-2-4-6-8/h7-8H,1-6H2 |
Std. InChIKey | KDYFGRWQOYBRFD-UHFFFAOYSA-N.XXMIOPMDWAUFGU-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 1741 | |
Density ρ | g mL-1 | 1.151 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 220 | 220 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
1Extrapolated value
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 200.23 | |
Van-der-Waals Volume VvW | mL mol-1 | 112 | |
Molar Volume Vm | mL mol-1 | 168 - 172 | 170 |
Density ρ | g mL-1 | 1.17 - 1.19 | 1.18 |
Solubility Parameter δ | MPa1/2 | 19.0 - 20.3 | 19.7 |
Molar Cohesive Energy Ecoh | J mol-1 | 60500 - 70800 | 66100 |
Glass Transition Temperature Tg | K | 204 - 246 | 221 |
Molar Heat Capacity Cp | J (mol K)-1 | 373 - 382 (l) | 378 |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.48 - 1.49 | 1.49 |
Last updated: November 23, 2017