POLYMER CLASS | Polyhaloolefins |
COMMON NAMES | Poly(chlorotrifluoroethylene) |
STRUCTURE BASED NAME | Poly(1-chloro-1,2,2-trifluoroethylene) |
ACRONYMS | PCTFE, PTFCE |
CAS # | 9002-83-9 |
CurlySMILES | C{-}(Cl)(F)C{n+}(F)(F) |
CAS # | 9036-80-0 |
COMMON NAMES | Chlorotrifluoroethene |
SMILES | FC(=C(F)F)Cl |
Std. InChI | InChI=1S/C2ClF3/c3-1(4)2(5)6 |
Std. InChIKey | UUAGAQFQZIEFAH-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 56.0 - 60.7 | 58.3 |
Density ρ | g mL-1 | 1.92 - 2.08 | 2.00 |
Solubility Parameter δ | MPa1/2 | 14.7 - 16.2 | 16.0 |
Molar Cohesive Energy Ecoh | J mol-1 | 13100 - 15900 | 15500 |
Glass Transition Temperature Tg | K | 318 - 423 | 360 |
Molar Heat Capacity Cp | J (mol K)-1 | 97.6 - 104.7 | 101.1 |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.39 - 1.57 | 1.42 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 116.47 | |
Van-der-Waals Volume VvW | mL mol-1 | 34.48 | |
Molar Volume Vm | mL mol-1 | 52.8 - 60.2 | 56.0 |
Density ρ | g mL-1 | 1.93 - 2.21 | 2.08 |
Solubility Parameter δ | MPa1/2 | 13.4 - 18.6 | 16.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 10700 - 18200 | 14500 |
Glass Transition Temperature Tg | K | 307 - 458 | 365 |
Molar Heat Capacity Cp | J (mol K)-1 | 102.1 - 103.7 | 103.2 |
Entanglement Molecular Weight Me | g mol-1 | 6100 - 16200 | 11100 |
Index of Refraction n | none | 1.40 - 1.46 | 1.44 |
Last updated: August 7, 2016