POLYMER CLASS | Polymethacrylamides |
COMMON NAMES | Poly(N-tert-butylmethacrylamide) |
STRUCTURE BASED NAME | Poly[N-(tert-butyl)aminocarbonyl-1-methylethylene] |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(C)(C(=O)NC(C)(C)C) |
CAS # | 6554-73-0 |
COMMON NAMES | n-tert-butylmethacrylamide |
SMILES | CC(=C)C(=O)NC(C)(C)C |
Std. InChI | 1S/C8H15NO/c1-6(2)7(10)9-8(3,4)5/h1H2,2-5H3,(H,9,10) |
Std. InChIKey | QQZXAODFGRZKJT-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 138.0 | |
Density ρ | g mL-1 | 1.02 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 433 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 141.21 | |
Van-der-Waals Volume VvW | mL mol-1 | 89.4 | |
Molar Volume Vm | mL mol-1 | 137.2 - 139.3 | 138.4 |
Density ρ | g mL-1 | 1.01 - 1.03 | 1.02 |
Solubility Parameter δ | MPa1/2 | 21.6 | |
Molar Cohesive Energy Ecoh | J mol-1 | 64600 | |
Glass Transition Temperature Tg | K | 422 - 453 | 437 |
Molar Heat Capacity Cp | J (mol K)-1 | 208 - 225 | 213 |
Entanglement Molecular Weight Me | g mol-1 | 33000 - 34700 | 33800 |
Index of Refraction n | none | 1.50 - 1.53 | 1.50 |