POLYMER CLASS | Polycarbonates |
COMMON NAMES | Poly(2,6,3',5'-tetrachloro bisphenol A carbonate) |
STRUCTURE BASED NAME | Poly[oxycarbonyloxy(2,6-dichloro-1,4-phenylene)(dimethylmethylene)(3,5-dichloro-1,4-phenylene)] |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}(=O)Oc1c(Cl)cc(cc1Cl)C(C)(C)c2cc(Cl)c(c(Cl)c2)O{n+} |
CAS # | |
COMMON NAMES | 4,4'-Propane-2,2-diylbis(2,6-dichlorophenol), Phosgene |
SMILES | CC(c1cc(Cl)c(c(c1)Cl)O)(c1cc(Cl)c(c(c1)Cl)O)C.ClC(=O)Cl |
Std. InChI | 1S/C15H12Cl4O2/c1-15(2,7-3-9(16)13(20)10(17)4-7)8-5-11(18)14(21)12(19)6-8/h3-6,20-21H,1-2H3 . 1S/CCl2O/c2-1(3)4 |
Std. InChIKey | KYPYTERUKNKOLP-UHFFFAOYSA-N.YGYAWVDWMABLBF-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | ||
Density ρ | g mL-1 | ||
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 493 - 504 | 500 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.59 - 1.61 | 1.60 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 250.25 | |
Van-der-Waals Volume VvW | mL mol-1 | 172.1 | |
Molar Volume Vm | mL mol-1 | 264.2 - 280.1 | 272.2 |
Density ρ | g mL-1 | 0.89 - 0.95 | 0.92 |
Solubility Parameter δ | MPa1/2 | 19.6 - 22.0 | 20.6 |
Molar Cohesive Energy Ecoh | J mol-1 | 107400 - 128200 | 115300 |
Glass Transition Temperature Tg | K | 461 - 496 | 496 |
Molar Heat Capacity Cp | J (mol K)-1 | 360.0 - 389.1 | 374.4 |
Entanglement Molecular Weight Me | g mol-1 | 2500 - 5700 | 3970 |
Index of Refraction n | none | 1.57 - 1.62 | 1.59 |