Poly[oxy(hexyloxymethyl)ethylene]
CROW logo
Poly[oxy(hexyloxymethyl)ethylene]
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyglycol
COMMON NAMESPoly[oxy(hexyloxymethyl)ethylene]
STRUCTURE BASED NAME Poly(2-(hexoxymethyl)oxirane), Poly(3-hexoxypropylene oxide)
ACRONYMS  
CAS #  
CurlySMILES O{-}C(COCCCCCC)C{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 5926-90-9
COMMON NAMES 2-(Hexoxymethyl)oxirane
SMILES CCCCCCOCC1CO1
Std. InChI 1S/C9H18O2/c1-2-3-4-5-6-10-7-9-8-11-9/h9H,2-8H2,1H3
Std. InChIKey JPEGUDKOYOIOOP-UHFFFAOYSA-N
STRUCTURE
2-(Hexoxymethyl)oxirane
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 164 
Density ρg mL-1 0.97 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK 188 - 190189
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.47  
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 158.24
Van-der-Waals Volume VvWmL mol-1 96.5
Molar Volume VmmL mol-1 153 - 168161
Density ρg mL-1 0.94 - 1.040.98
Solubility Parameter δMPa1/2 17.4 - 18.517.8
Molar Cohesive Energy EcohJ mol-1 49900 - 5250051000
Glass Transition Temperature Tg K 184 - 207 199
Molar Heat Capacity CpJ (mol K)-1 324 - 342334 (l)
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.471.47

  Last updated: August 13, 2016