Poly(1-ethyl-1,4-butadiene)
CROW logo


       
Poly(1-ethyl-1,4-butadiene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polydienes
COMMON NAMESPoly(1-ethyl-1,4-butadiene)
STRUCTURE BASED NAME Poly(1-ethyl-but-1-ene-1,4-diyl)
ACRONYMS
CAS #
CurlySMILES C{-}(CC)=CCC{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 592-48-3
COMMON NAMESHexadiene
SMILES CCC=CC=C
Std. InChI 1S/C6H10/c1-3-5-6-4-2/h3,5-6H,1,4H2,2H3
Std. InChIKey AHAREKHAZNPPMI-UHFFFAOYSA-N
STRUCTURE
Hexadiene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume Vm mL mol-1 92.2
Density ρg mL-1 0.89 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK 197 
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-16900 - 78007400
Index of Refraction nnone   
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 82.14
Van-der-Waals Volume VvWmL mol-1 59.23
Molar Volume VmmL mol-1 88.6 - 92.690.6
Density ρg mL-1 0.89 - 0.930.91
Solubility Parameter δMPa1/2 17.0 - 17.317.2
Molar Cohesive Energy EcohJ mol-1 26500 - 2720026800
Glass Transition Temperature TgK 184 - 201194
Molar Heat Capacity CpJ (mol K)-1 164.6 - 165.6165.2 (l)
Entanglement Molecular Weight Meg mol-1 3600 - 11200 6400
Index of Refraction nnone 1.46 - 1.511.49

  Last updated: May 7, 2018