Thermo-Physical Properties: Calculated Data
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 |
204.21 | |
Van-der-Waals Volume VvW | mL mol-1 |
| |
Molar Volume Vm | mL mol-1 |
| |
Density ρ | g mL-1 |
| |
Solubility Parameter δ | MPa1/2 |
| |
Molar Cohesive Energy Ecoh | J mol-1 |
| |
Glass Transition Temperature Tg | K |
343 | |
Molar Heat Capacity Cp | J (mol K)-1 |
| |
Entanglement Molecular Weight Me | g mol-1 |
| |
Index of Refraction n | none |
1.48 | |
*The properties depend on the number of methoxy groups on the repeating glucose units. The methoxy degree of substitution is typically in the range of 2.0.